The MDMT of the vessel is -45 deg C. The vessel is 2" thick. material A 516 Gr 70 (Impact tested at -46 Deg C).
The main seams (Category A, B, C, D)are welded with GMAW and GMAW +SAW Combination. (All Groove PQRs Impact tested at -46)
The externals (Ladder, Platform) Fillets are welded with SMAW and FCAW.
Is it mandatory to have Groove Qualification (For Impact)
or Is it OK to have just Fillet Qualification for SMAW and FCAW.
Code of Construction ASME Sec VIII Div 1. Qualification done to ASME Sec IX.
Project or Purchase/Client Spec does not address the above issue.
Is there an explicit reference in ASME Sec VIII Div 1 or In Sec IX that calls for impact test qualification, when only fillet is involved.
The main seams (Category A, B, C, D)are welded with GMAW and GMAW +SAW Combination. (All Groove PQRs Impact tested at -46)
The externals (Ladder, Platform) Fillets are welded with SMAW and FCAW.
Is it mandatory to have Groove Qualification (For Impact)
or Is it OK to have just Fillet Qualification for SMAW and FCAW.
Code of Construction ASME Sec VIII Div 1. Qualification done to ASME Sec IX.
Project or Purchase/Client Spec does not address the above issue.
Is there an explicit reference in ASME Sec VIII Div 1 or In Sec IX that calls for impact test qualification, when only fillet is involved.