I have an older part and a newer part built from the same mold. Resin batches were obviously not the same. New parts all crack easily.
My first question is; was the correct resin used? Can PBTGF30 be compared and identified from Sabic, 3M, BASIF, Dupont?
Would the FTIR test be a good choice? Sabic Valox 470 PBTGF30 was the resin on the drawing, but I am not clear how to verify if this was the one used.
How would you compare the parts for mold parameters? IE would the hardness test reveal this? Other suggestions?
My problem here;
The parts were last molded in 2007. Today it is my problem to figure out why they are different. The supplier is not the same for both parts, but the mold is the same (on a different machine, with a new guy driving it). Latest supplier doesn't have records of the mold parameters apparently.
My first question is; was the correct resin used? Can PBTGF30 be compared and identified from Sabic, 3M, BASIF, Dupont?
Would the FTIR test be a good choice? Sabic Valox 470 PBTGF30 was the resin on the drawing, but I am not clear how to verify if this was the one used.
How would you compare the parts for mold parameters? IE would the hardness test reveal this? Other suggestions?
My problem here;
The parts were last molded in 2007. Today it is my problem to figure out why they are different. The supplier is not the same for both parts, but the mold is the same (on a different machine, with a new guy driving it). Latest supplier doesn't have records of the mold parameters apparently.