I am studying tube - tubesheet connection during hydraulic expansion.
I used Podohrsky book and I understood how to calculate the limiting pressure and adesion pressure but I don't understand how to calculate the pressure when tubesheet starts with plastic deformation.
My idea is to use equation 5.8 for tubes and use UP instead of ur with yield strenght of tubesheet, is that okay?