How to etch heat treated spring steel for observing prior austenite grain size (AGS) 1

Status
Not open for further replies.

Best99

Materials
Joined
Sep 22, 2008
Messages
17
Location
TH
Dear all,

After quenching and tempering. I did the tempering at 500℃x24hr for grain boundary embrittlement.Then etched by this solution

1. Saturated picric solution 50 ml (4g picric acid mix with water)
2. Surface-active-agent, Sodium dodecylbenzensulfonate 5ml
3. HCL 1.0ml

As a result, I cannot get clearly AGS as well.

Could you please guide me the how to get clearly AGS step by step

Thank you for your comment
 