the job description:
the material is steel 1010, parts are 1 1/4 inch washer. heating 1 hour at 1650F in carbonitride atomsphere. then quench in 90F poplymer. without tempering.
the test on the parts after heat treating shows porosity under the surface.
the question: why porocity happens? and what we can do to make it disappear?
thanks
yush
the material is steel 1010, parts are 1 1/4 inch washer. heating 1 hour at 1650F in carbonitride atomsphere. then quench in 90F poplymer. without tempering.
the test on the parts after heat treating shows porosity under the surface.
the question: why porocity happens? and what we can do to make it disappear?
thanks
yush