We deal with the design of pipe systems for steam and brine (geothermal gathering system) following B31.1 (we use Coade CaesarII to design) we have new applications that use bigger diameters, our worst cases are 60" diam, with a thickness defined by internal presure of 3/8" (D/t=160) and other of D:50" t:5/16" (D/t=160) with lenghts of the order of 300 ft or more installed in cross country.
Our design condition is internal pressure 131psig (9 barg) and 356°F (180°C) and we plan to use ASTM A515 Gr.70 plate.
We are looking for criteria about such dimensiones and how to define when D/t ratios start to need special considerations such as stiffner rings, use bigger thickness, etc., considering high loads on supports and high loads on "Ts" and "Ys" could be spected.
So I´d appreciate if somebody can give some hints on where to find criteria on this or somebody has been related with similar cases and if he has used special considerations, or anny comment on this.
Thanks a lot in advance, and blessings to you all from Costa Rica.
Our design condition is internal pressure 131psig (9 barg) and 356°F (180°C) and we plan to use ASTM A515 Gr.70 plate.
We are looking for criteria about such dimensiones and how to define when D/t ratios start to need special considerations such as stiffner rings, use bigger thickness, etc., considering high loads on supports and high loads on "Ts" and "Ys" could be spected.
So I´d appreciate if somebody can give some hints on where to find criteria on this or somebody has been related with similar cases and if he has used special considerations, or anny comment on this.
Thanks a lot in advance, and blessings to you all from Costa Rica.