I have a client that wants to put a doorway in a load bearing wall. The wall, 18 inch thick concrete, engineered and built in 1963, has reinforcing steel but I do not know how much. <br>
<br>
I could make the opening and use the steel to meet requirements but I do not know how to identify it without breaking the wall header apart. Are there any good techniques for 1) finding the old engineering drawings, and 2) measuring the existing steel content of this wall?<br>
<br>
<br>
I could make the opening and use the steel to meet requirements but I do not know how to identify it without breaking the wall header apart. Are there any good techniques for 1) finding the old engineering drawings, and 2) measuring the existing steel content of this wall?<br>