Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Plasma cutting steel plate in preparation for fabricating multi-sided monopoles

Status
Not open for further replies.

VoyageofDiscovery

Structural
Joined
Apr 7, 2002
Messages
619
Location
CA
As plasma cutting is relatively new, I think this may be why I don't see much reference to plasma cutting in current Steel and Welding Codes.

I am wondering if there are any thoughts out there on how it would affect the long-term performance of such structures?

VoD
 
Companies like Valmont have been plasma-cutting (both the steel plate used to fold into tubes and the various vangs and attachments) for many years. It should be a better end condition than shearing, especially if the edges are ground for standard weld prep.
 