I have an application where we are using a nichrome v wire to move a contact. We have a mechanical adjustment to allow calibration of the contact. The calibration however when set during the day, and then verified the next day changes. We bake the unit containing the nichrome wire at 220 deg F for 12 hours. I think this is an attempt to stress relieve or stablize the nichrome wire. Does anyone know what temp would stress relieve the nichrome v wire?