I'm trying to get 1.5 mm AA5754-O sheet to 19% minimum uniform elongation (consistently) while maintaining 105 MPa yield minimum. I can easily get one without the other, of course. I can get both, on occasion, but it's not consistent from sample to sample. At the very best, the yield strength is always borderline on the low side and the uniform elongation is borderline as well. Discontinuous yielding complicates the matter by adding to the variability of the uniform elongation results. I'd like to be "safely" within the specification. I've tried chemistry changes and rolling practice changes, and I've experimented with final anneal temperatures (within the limits of a batch furnace), but so far nothing has worked. I'm sure there are many things to consider, and I know I'm probably not giving enough info for specific answers at this stage, but I need to get some guidance and suggestions on which direction to take. Unfortunately, I don't have an R&D department or an extensive list of in-house technical resources on-hand, so I'm hoping there are some knowledgeable folks out there who can help! I'm certain someone out there is very familiar with this issue.