Australia has AS/NZS 4673 'Cold-formed stainless steel structures'. There is no code for hot-rolled stainless steel.

Perusing AS 4100 'SCOPE AND APPLICATION' it stipulates 'This Standard applies to buildings, structures and cranes constructed of steel' (refer attached). Is is therefore satisfactory that hot-rolled stainless steel sections satisfying all the other constraints in that clause be designed to AS 4100?
Rgds
 
 http://files.engineering.com/getfile.aspx?folder=fe85f47f-fce5-45af-92c9-87ff5dc50134&file=AS4100_SCOPE_excerpt.jpg
Replies continue below

Recommended for you

Don't know about Australia but in the US the AISC doesn't deal with stainless steel.

Check out Eng-Tips Forum's Policies here:
faq731-376
 
AISC has a design guide (I think it's Design Guide 27). Some design equations are modified but they mostly refer back to AISC 360.
 
From the design guide:
The major difference between the mechanical properties of carbon and stainless steel is the stress-strain relationship - stainless steel has a continuous, but nonlinear, relationship between stress and strain.

It goes on to mention that the Design Guide is based on the provisions in the European Design Manual fro Structural Stainless Steel and Eurocode 3: Design of Steel Structures, Supplementary Rules for Stainless Steel, Part 1-4.
 
Thanks all for your inputs. Appreciate your comments.