The insulation and covers can be problematic at flanges.
Make sure that these are well installed.
The Zn will hold up well if protected and dry.
It is good to add to your piping inspection to check for rust bleeding from the drain holes at flanges.
It either means that your flange seal is leaking, or you have gotten water into the flange.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed