Is it possible hot bending safely 1" Sch 80 pipe(material: Incoloy 800H)?
 
Replies continue below

Recommended for you

tanocba;
Yes, this material can be subjected to hot bending. I would suggest you visit the web site below and review background information for this material. In addition, you should perform a solution heat treatment after tube bending to restore elevated temperature properties and corrosion resistance.

 