Please guide me what material and type of hose is suitable for Lime slurry application with 90 Deg C temp and with 160 PSI pressure. My specification further says 3:1 refers RMA standards

Please help!
 
Replies continue below

Recommended for you

Depending upon the hose size and length I would not see any problem in using a standard rubber hydraulic hose with steel reinforcement. They are cheap for small sizes and you will get them everywhere. And their pressure rating exceeds your requirement by far.
 
Hi Micalbrch, Thanks for the headsup...

Do you suggest me any specific references so I can keep a basis for my selection ..thanks in advance!

 