I want to provide a horizontal construction joint in a wall. There is a lap splice of the reinforcement at the same height. I think that the continuity of the steel will be established whether or not the wall is placed in lifts or monolithically.
Will the transfer of force between bars by bond stress be affected if I locate a horizontal construction joint in a wall where the reinforcing steel is lap spliced? Is this permitted by ACI? Has anyone done this before?