Any idea on what resins I can use to withstand strong fragrances that contains citrus & aldehyde?
I've tried PS, PETG, PETE, PETG, PCTG, they have all failed, I was told there may be some PETE polymer blend or high clarity PP material that might work?
HELP!!!
I've tried PS, PETG, PETE, PETG, PCTG, they have all failed, I was told there may be some PETE polymer blend or high clarity PP material that might work?