Joint is a 6 bolt joint and soft one with a gasket in between. We are using torque control angle monitor shut off strategy.
Torque – 240-260 in-lbs
Angle shut off monitor limit – 750 deg
Snug – 25 in-lbs (random guess)
We are using 750 deg monitor because the very first bolt in that soft joint always shows high angles to achieve the target torque of 250 in-lbs and the rest of them something below 750 as the joint gets stiffer and stiffer after each bolt is tightened.
But for some reason we are getting high angles of more than 750 deg on some bolts and the tool shuts off and the torque achieved is very low, some thing in the range of 40-100 in-lbs. I know this generally occurs when something in the joint is deformed. I check for bolt and joint deformation but nothing occurred.
Any ideas?