Nov 8, 2019 #1 PhenolicComp Aerospace Joined Nov 8, 2019 Messages 1 Location US Hi. I have some problem on bagging my phenolic resin. It always blow up during autoclave cure. Anyone have the same issue? Any ideas ob how to properly bag phenolic resin? Thank you.
Hi. I have some problem on bagging my phenolic resin. It always blow up during autoclave cure. Anyone have the same issue? Any ideas ob how to properly bag phenolic resin? Thank you.
Nov 8, 2019 #2 ewh Aerospace Joined Mar 28, 2003 Messages 6,149 Location US I suggest asking to delete this thread and posting here -> forum327 You're more likely to get better responses. "Know the rules well, so you can break them effectively." -Dalai Lama XIV Upvote 0 Downvote
I suggest asking to delete this thread and posting here -> forum327 You're more likely to get better responses. "Know the rules well, so you can break them effectively." -Dalai Lama XIV
Nov 8, 2019 #3 IRstuff Aerospace Joined Jun 3, 2002 Messages 44,895 Location US You should be able to delete it yourself. TTFN (ta ta for now) I can do absolutely anything. I'm an expert! https://www.youtube.com/watch?v=BKorP55Aqvgfaq731-376 forum1529 Entire Forum list http://www.eng-tips.com/forumlist.cfm Upvote 0 Downvote
You should be able to delete it yourself. TTFN (ta ta for now) I can do absolutely anything. I'm an expert! https://www.youtube.com/watch?v=BKorP55Aqvgfaq731-376 forum1529 Entire Forum list http://www.eng-tips.com/forumlist.cfm
Nov 8, 2019 #4 GregLocock Automotive Joined Apr 10, 2001 Messages 23,890 Location Orbiting a small yellow star I don't do that forum. You probably need to de-aerate your resin before use by ultrasonic shaking under a vacuum. Cheers Greg Locock New here? Try reading these, they might help FAQ731-376 http://eng-tips.com/market.cfm? Upvote 0 Downvote
I don't do that forum. You probably need to de-aerate your resin before use by ultrasonic shaking under a vacuum. Cheers Greg Locock New here? Try reading these, they might help FAQ731-376 http://eng-tips.com/market.cfm?
Nov 8, 2019 #5 Compositepro Chemical Joined Oct 22, 2003 Messages 7,841 Location US https://www.eng-tips.com/viewthread.cfm?qid=454481 https://www.eng-tips.com/viewthread.cfm?qid=453968 Upvote 0 Downvote
https://www.eng-tips.com/viewthread.cfm?qid=454481 https://www.eng-tips.com/viewthread.cfm?qid=453968