Hi everybody
I am trying to calculate the required equivalent thickness of a vessel using IMDG 6.7.2.4.7 code but the value I get is way too small.
I need help on how the formula works.
The formula is
e1 = 21.4e0d/(1.8(Rm*A1)^1/3)
e0 = 6mm
d = 2.075m
Rm = 485MPa
A1 = 40%
Thank you
I am trying to calculate the required equivalent thickness of a vessel using IMDG 6.7.2.4.7 code but the value I get is way too small.
I need help on how the formula works.
The formula is
e1 = 21.4e0d/(1.8(Rm*A1)^1/3)
e0 = 6mm
d = 2.075m
Rm = 485MPa
A1 = 40%
Thank you