1.)
20160427_193047_1_wfty4e.jpg

microestructure of a 1018 steel. water quenched. nital 2% etch during 5 seconds, 100X.


2.)
A)
20160426_145149_1_bs6i0r.jpg

microestructure of a 1018 steel. oil quenched. using nital 5% etch during 5 seconds, 100X.

B)
20160426_144809_1_v8dcig.jpg

microestructure of a 1018 steel. oil quenched. using nital 5% etch during 5 seconds, 10X. (use zoom to watch better)

3.)
20160420_200806_1_nk5iey.jpg

microestructure of a 1018 steel. brine quenched. picral 4% etch during 5 seconds, 100X.
 
Replies continue below

Recommended for you

As a general description, I would say overexposed with too little contrast.

How are you taking these pictures? They look as if they were taken with a phone through the eyepiece of a microscope.

What are you trying to accomplish? How you describe the microstructure depends on what you are trying to illustrate.
 
Look like low carbon lath martensite to me....
 