I was wondering if anyone can help me indentify this material. It is used in High temperature automotive applications as a bushing.

C = 1.139
Mn = .540
P = .041
S = .021
Si = 2.149
Cr = 32.812
Ni = .377
Mo = 2.054
Cu = .228
Mg = .032
W = .039
V = .277
Co = .053
Sn = .012
Al = .034
Nb = .049
Pb = .007
B =.004
Se = .002
Ta = .002
Zr = .010
Fe = Remainder

Thanks

 
It is a tool steel due to high carbon content 1.1%,Grade, I shall have to look up and let you know,or you could do that yourself now.
 
This does not resemble a conventional wrought alloy. Any chance that the current part is made by a powder metallurgy process (PM)? Or that the part has a coating, rendering the composition as a composite of the base metal + coating? Materials used near the exhaust side of automotive cylinder heads are often made by PM methods and/or use hard coatings such as Stellite.
 

It does have black coating, we figured it was nitrided.

Given so much Carbon, that hardness was only 38 HRC, which I thought was odd.



The PM comment is very interesting, as another part we have I swore is PM but it is made up of CK20 which is an investment cast 310 stainless. I am unsure if the PM composition would be the same as the cast, or would it resemble the wrought alloy more.

 
Were it not for the carbon content, it looks like the ferritic stainless SHOMAC 30-2 that's listed in my copy of the Metals Handbook. Add a carbide coating?
 
Are you sure you have Ni and Fe the right way around? Or swap Fe and Co and it looks like F75.

If that is a steel, it would have to be made to order by a specialist alloy supplier, it doesn't seem to fit any of the international specs.
 