I was wondering if anyone can help me indentify this material. It is used in High temperature automotive applications as a bushing.
C = 1.139
Mn = .540
P = .041
S = .021
Si = 2.149
Cr = 32.812
Ni = .377
Mo = 2.054
Cu = .228
Mg = .032
W = .039
V = .277
Co = .053
Sn = .012
Al = .034
Nb = .049
Pb = .007
B =.004
Se = .002
Ta = .002
Zr = .010
Fe = Remainder