zhlin,
I have the spec with me,which specifies the austenitizing temperature as 1550F(845C), liquid media quenched to below 500F(260C) and then tempered at 1100F(595C).
Why have you gone for such a long austenitizing cycle ( I am assuming,as you have not mentioned)?
Learn the rules,so you know how to break them properly.