Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Heat exchanger: welds between plates in ASME SA 387 Gr.91 and other components in Gr.9

Status
Not open for further replies.

FPPE

Mechanical
Joined
Mar 4, 2022
Messages
196
Location
IT
Hi,

Our customer asked us to make a complete exchanger in Gr.9, but the plates in SA 387 Gr.9 cannot be used because the allowable values are not tabulated in the ASME IID.
I would know (and in the case it would not be possible understand why) if it is possible to weld the plates in ASME SA 387 Gr.9 with girth flanges and nozzles respectively in ASME SA 182 F9 and ASME SA 335 P9.

Thank you in advance
 
I suppose it would be possible to weld those materials, but with the assembly not Code compliant. Is there some reason you cannot use plate SA-397 Gr 91? Permitted under Sec 1, Sec VIII, Div 1 and Sec III at 3" thickness or less.

Regards,

Mike