The hardness at is shown as “23-27 R ASTM E384-89.”
I am assuming that the "R" is Rockwell R, which cannot be measured by ASTM test method E384 (Knoop, Vickers).
Perhaps the measurements were made in accordance with ASTM E384 and then translated into what they thought was the equivalent Rockwell R value.
Is there a formula for converting Vickers to Rockwell R?
I am assuming that the "R" is Rockwell R, which cannot be measured by ASTM test method E384 (Knoop, Vickers).
Perhaps the measurements were made in accordance with ASTM E384 and then translated into what they thought was the equivalent Rockwell R value.
Is there a formula for converting Vickers to Rockwell R?