How do we check Hardness values for Graphite Block - Is it Rockwell C scale or Rockwell B scale. Which is better
 
What is the spec? What does it say?


= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Rockwell L perhaps.

Check the standard as mentioned below for more......

ASTM C748 - 20
Standard Test Method for Rockwell Hardness of Graphite Materials

DHURJATI SEN
Kolkata, India

 
Thanks for the inputs
 