shamrock138
Mechanical
Hello All,
I am currently on a project that the customer wants hardness testing done on existing PQR's. I have duplicated one of the original test coupons for a PQR, but I am having a hard time finding SA-285 Gr. C 3/8" thick for the second coupon, which was the original material and thickness used for approval. Does the material and thickness have to be identical to the original PQR or can I use a material with equal or greater properties?
Any help would be greatly appreciated.
I am currently on a project that the customer wants hardness testing done on existing PQR's. I have duplicated one of the original test coupons for a PQR, but I am having a hard time finding SA-285 Gr. C 3/8" thick for the second coupon, which was the original material and thickness used for approval. Does the material and thickness have to be identical to the original PQR or can I use a material with equal or greater properties?
Any help would be greatly appreciated.