LCform
Mechanical
- Jan 13, 2016
- 139
Hi All
I was wondering which test is better and if there are appropriate devices to measure the hardness on the bolts cylindrical part, since with the brinel test device that we have it's not possible, I was thinking of HV , but I am not sure, I wanted to sample the hardness on different parts, from flat to rounded , but the dimensions are sometimes small , at the order of 10 mm diameter
what do you suggest me
Thank you very much
I was wondering which test is better and if there are appropriate devices to measure the hardness on the bolts cylindrical part, since with the brinel test device that we have it's not possible, I was thinking of HV , but I am not sure, I wanted to sample the hardness on different parts, from flat to rounded , but the dimensions are sometimes small , at the order of 10 mm diameter
what do you suggest me
Thank you very much