Hi guys,

I would like to ask if an H beam structure EN10025 S355JR would be applicable for -20deg C or lower temperature area?

Thank you very much.
 
hi steve,

Thank you for your reply I would just like to clarify, does it means that this values from the impact test temperatures will define which temperature I can build or use a certain structure?
 