Can someone shed some light on why in EN ISO 15614-1 hardness survey is not required for stainless steels in group 8?
Hardness Survey is not required for :-
Steels in Sub-group 1.1 (yield strength of 275N/mm2 or less)
Stainless Steels in Group 8
Nickel Alloys in Groups 41 to 48
Hardness Survey is not required for :-
Steels in Sub-group 1.1 (yield strength of 275N/mm2 or less)
Stainless Steels in Group 8
Nickel Alloys in Groups 41 to 48