I have some ball valves in my system that have started to exhibit higher torque requirements to actuate. I took a couple apart to see what was going on, and noticed that the stem and O-rings seemed rather "dry". The grease appeared to lose all it's lubricating qualities, although it was obvious that it was still there.

The manufacturer says the valves are made with a synthetic grease (Kluebersynth VR 69-252) and EPDM O-rings. We used a sodium nitrite based corrosion inhibitor on the system. Our medium is ethylene glycol/water (50/50).

Is it possible one of these chemicals is reacting with the grease to cause this "drying out"? Any suggestions for other types of grease?
 
Replies continue below

Recommended for you

Yeckelch,
try consulting the websites mentioned in Thread408-104579: maybe you'll find some information about the lubricants' chemical compatibilty...
Bye, 'NGL
 