Graphics on a stainless steel container

Status
Not open for further replies.

Harini Krishna

Electrical
Joined
Jan 7, 2020
Messages
25
Location
IN
Hi,
Can you tell me how to make gradient graphic design made in the image given below on a stainless steel container?

vaya_awpfjm.png


Thankyou
 
IRstuff,
Thank you for the reply.
Can you tell me how the design on the container is made during the manufacturing process?
 
A few methods:

It's printed on much like an ink jet printer.

Or, The background gradient is painted on using a series of paint nozzles and then the lattice pattern is rolled on.

Or, It's a vinyl wrap.


 
based on their website's "specs" it's a powder coating, which is probably the only thing that can withstand the handling environment.

TTFN (ta ta for now)