Are there any metallurgical reasons why I shouldn't use ASTM A194 Grade 3 nuts (what we bought) instead of Grade 4 (what is currently in place) on some external bolts for heat exchangers in diesel hydrotreater service provided they meet the code requirements for the service?
 
Replies continue below

Recommended for you

Seems to me that a more germane question might be that if "grade 3" bolts "meet the code requirements for the service" why were grade 4 bolts ordered?

There must have been some difference to warrant the grade 4, so what's changed now, that you can specify grade 3?

TTFN

FAQ731-376
Chinese prisoner wins Nobel Peace Prize
 
There is a significant difference between Grade 3 and Grade 4 nuts.

Grade 3 - 5% Cr- 0.5% Mo, more for higher temperature applications

Grade 4 - is a carbon-molybdenum (0.25%) steel.

The major difference will be increased corrosion performance by the higher chromium steel.

 