Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

GD&T of magnets

Status
Not open for further replies.

stoicFN

Mechanical
Joined
Nov 30, 2007
Messages
1
Location
US
Can anyone tell me the proper way to GD&T magnets with their orientation, polarization, etc., or where I might be able to track down such information? Thanks!!


-Fred
 
Just do GD&T on the physical part. There isn't GD&T for orientation and polarization. You may need a note for grain direction, depending on the material.

Chris
SolidWorks 08 0.0/PDMWorks 08
AutoCAD 06
ctopher's home (updated 10-07-07)
ctopher's blog
 
Fred,

As Chris mentioned, I do not believe there is symbology for magnetism in mechanical drafting, but there may be some in electrical drafting. Don't a bried yahoo search, I found this link that may point you in the right direction:


It's dealing with electro-magnets, but may have some clues to answer your question.


Matt Lorono
CAD Engineer/ECN Analyst
Silicon Valley, CA
Lorono's SolidWorks Resources
Co-moderator of Solidworks Yahoo! Group
and Mechnical.Engineering Yahoo! Group
 
Here are some notes that I put on my last drawing for a Neodymium magnet.

Magnets Rare-Earth Neodymium-Iron-Boron Magnet

Shape - Disc

Dimension - Diameter 0.250" (6.35mm) x Thickness 0.100" (2.54mm)

Material - Sintered NdFeB

Magnetization - Magnetized

Magnetization Direction - Axially Magnetized

Plating – Nickel

Temperature Range (Deg C) - 0 to 80

Dimensional Tolerance - (+/-0.005")

Grade N30

Pull Force - 2.14lb/971g


Heckler [americanflag]
Sr. Mechanical Engineer
SWx 2007 SP 4.0 & Pro/E 2001
o
_`\(,_
(_)/ (_)

This post contains no political overtones or undertones for that matter and in no way represents the poster's political agenda.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top