Apparently, this column is being used as a downspout and is clogged..


IMG_2638_rchy75.jpg
 
I used to shop at the "Day Old Dough Flour" store.
 
1503-44,

Wouldn't uncontrolled, uneven hydration a concern?
 
Gas station canopies are the first thing you see flying down the road in those severe weather videos.

The second thing is PEMBs being ripped apart.
 
JLNJ, for a lot of reasons, I got to go to the Florida Keys after Irma and the panhandle after Michael. You are exactly correct. In a rough order, excluding residential:
[ul]
[li]Gas Station Canopies[/li]
[li]Fast Food establishments (lots of glass, inexpensively designed and constructed)[/li]
[li]PEMB's[/li]
[li]Light Poles (lots of leaners)[/li]
[/ul]

 
R13, we mix prior to. canwesteng mentioned powder.

 
@Jed

The other part of my observation about the flimsiness of gas station canopies is that either we don’t understand the complex action of wind on these types of structures or the people who design them don’t design with the natural robustness as is seen in “normal” structures.

Maybe it’s just the commercial pressure to make these things as cheap as possible.

 
As soon as you mix the cement with anything else, it no longer is cement. It can be grout, or concrete. But cement is specifically a dry powder used in combination with other materials to create a final product. Cement is an ingredient.
 
From Britannica:
"Cement, in general, adhesive substances of all kinds,"
One type of cement may be used to bind agregate together to form mortar or concrete.
A well casing may be "cemented" to the surrounding strata to prevent blowouts past the outside of the casing and to prevent the BOP and a section of casing heading skyward in extreme instances.
And enough of this cement will probably prevent the entry of water:
image_lowtrc.png


Bill
--------------------
"Why not the best?"
Jimmy Carter
 
I use it when connecting my PVC drain pipes. It is glue alike.
 
Fine. We still "cement" oil wells. If it makes you happier, think of "cement" as a verb. [bull]

 
1503-44,

Got you. I think either noun or verb is equally applicable to oil well related events.
 
Works for me. In fact, as long as you don't call it concrete, I'm happy as a clam in the mud.

 
It is a good absorbent and sealant in application with oil, I believe.
 
I assume you folks are arguing about Portland cement. There are many cementitious materials.

We structural engineers are a bit sensitive about our concrete buildings being called "cement" buildings.
 
Different industry uses the word differently. See the product addressed by Waross above, in piping practice, it is called "cement" rater than name it as glue, adhesive, or just sealant.
 
Yeah. I do know the difference. Actually my degree & PE is civil-structural. I started this doing wood roof trusses while in school. After graduating I did pipe stress (space frames) and heavy pump and compressor foundations, refinery pipe racks, 180' tall stair towers, pulp and paper conveyors, chem reactor fdtns, barge docks, helicopter pads on offshore plfms, Texas AM football stadium, some nuclear pipe work, then all of a sudden other opportunities opened up. Like they say, "Specialisation is for insects".

 
Like they say, "Jack of all Trades, Master of None"
 
That's also true, at least to some extent. You just have to maximise your transferable skill set. In my case it worked out well. Petroleum work is roughly divided into upstream, mid and downstream sectors and each tends to run in economic cycles. When oil is cheap, upstream work drops, but refinery and chemicals boom. Other industries like cheap oil too, so pulp and paper and mining work increases. Pipelines move the stuff all the time and the bulk of that work is civil, heavily combined with the ability to coordinate diverse work groups. Being able to do something useful in each, I almost always had more work than I wanted.

After a few years of doing the details, it usually turns out better in the long run to start supervising and project management and leave the finite element and CFD stuff to the kids. Let them work the simulators, keep them pointed in the right direction, correct their mistakes and push out practical designs, on time and sometimes even under budget.

And having broad experience and knowing how to use it turned out to be my most valuable asset, IMO, at least for projects that involve multiple disciplines and coordinating numerous and diverse organizations. You can always sub out complex design to vendors and specialist engineering companies. Never get caught out "Not seeing the forest for the trees".

 
I'll see your pissing column and raise you this.
IMG_20200923_170813_lwrj7g.jpg
 
$5 says someone cut out this slot in the column to replace the original internal drain once their column started pissing. Also a beautiful looking field splice (or something...?)! I'm sure the engineer was fully aware of all the mods.

gas_station2_ibovky.png
 
Status