Where can I find information regarding the strength of a friction welded joint between aluminum (6061-T6) and copper (cold-drawn)?

Thanks!
 
Replies continue below

Recommended for you

You might also try - they might give you a rough idea. But friction welds all have to be developed, metallurgically checked, bend tested etc on an individual basis. As a rough guide, it will be almost as strong as the aliminum.
 