Jun 5, 2003 #1 frayedknot Mechanical Joined May 23, 2003 Messages 18 Location US Where can I find information regarding the strength of a friction welded joint between aluminum (6061-T6) and copper (cold-drawn)? Thanks!
Where can I find information regarding the strength of a friction welded joint between aluminum (6061-T6) and copper (cold-drawn)? Thanks!
Jun 9, 2003 #2 Bove Aerospace Joined Apr 10, 2001 Messages 2 Location BR Try The Welding Institute : http://www.twi.co.uk...and good luck Upvote 0 Downvote
Jun 12, 2003 #3 EnglishMuffin Mechanical Joined May 21, 2003 Messages 1,103 Location US You might also try http://www.mtiwelding.com/ - they might give you a rough idea. But friction welds all have to be developed, metallurgically checked, bend tested etc on an individual basis. As a rough guide, it will be almost as strong as the aliminum. Upvote 0 Downvote
You might also try http://www.mtiwelding.com/ - they might give you a rough idea. But friction welds all have to be developed, metallurgically checked, bend tested etc on an individual basis. As a rough guide, it will be almost as strong as the aliminum.