Mar 17, 2025 #1 Drilling Integrity Super. Mechanical Joined Jun 26, 2024 Messages 3 Location SG Is there a formula that the ASME B31.3 code uses to calculate the Basic Allowable Stresses values in Table A-1?
Is there a formula that the ASME B31.3 code uses to calculate the Basic Allowable Stresses values in Table A-1?
Mar 21, 2025 #2 weldstan Materials Joined Jun 24, 2011 Messages 2,809 Location US I'm not sure what you are asking. Allowable stress is based on 1/3 of the specified minimum tensile strength of the material specification at room temperature up to specific defined higher temperatures. They are fully defined in B31.3.
I'm not sure what you are asking. Allowable stress is based on 1/3 of the specified minimum tensile strength of the material specification at room temperature up to specific defined higher temperatures. They are fully defined in B31.3.
Mar 21, 2025 #3 Geoff13 Structural Joined Oct 2, 2018 Messages 485 Location CA Are you looking for Clause 302.3.2?