Hello,
I would like to know if anyone has experiences in cutting a prolongation for 4130 forging before or after the final heat treatment.
Supplier proposes to me to cut before the final heat treatment the prolongation and put everything in the same batch for the heat treatment.
I have been told from supplier that, depends on thickness, cut after the final heat treatment can downgrade the material properties (which sound logical) and cut after final heat treatment will not permit to use the entire prolongation piece.
Do you have any experiences on that? if yes, which is the best solution for you?
Thanks
Rgds
Giuseppe
I would like to know if anyone has experiences in cutting a prolongation for 4130 forging before or after the final heat treatment.
Supplier proposes to me to cut before the final heat treatment the prolongation and put everything in the same batch for the heat treatment.
I have been told from supplier that, depends on thickness, cut after the final heat treatment can downgrade the material properties (which sound logical) and cut after final heat treatment will not permit to use the entire prolongation piece.
Do you have any experiences on that? if yes, which is the best solution for you?