Hello,
I am looking for some help in getting a ball park figure for a press fit. We are looking at high force linear servo motor from Rockwell to do the job. My problem is I'm not sure how much force is required. I have tried a few formulas I found on the web but the resulting answer was out of the ball park. I left the drawings at work but from what I can remember the details are:
Pin: .395" dia (solid), 303/304 S.S. .25 long
Mating hole: 12L14 steel, 52RC.
Maximum interference is .0018"
Any help would be greatly appreciated!!
I am looking for some help in getting a ball park figure for a press fit. We are looking at high force linear servo motor from Rockwell to do the job. My problem is I'm not sure how much force is required. I have tried a few formulas I found on the web but the resulting answer was out of the ball park. I left the drawings at work but from what I can remember the details are:
Pin: .395" dia (solid), 303/304 S.S. .25 long
Mating hole: 12L14 steel, 52RC.
Maximum interference is .0018"
Any help would be greatly appreciated!!