I have modeled axisymmetric analysis of sheet dome (simple push button).
I need to get the force response of the sheet metal. According to experimental results the force increases until certain level then the "spring" action occurs and the force drops a little bit and if you keep "pushing the button", the force increases very much. I am concerned about the force drop range.
However I keep getting steadily increasing force curve from the surface nodes (NFORC). Actually except one node all indicates the behavior similar to the experimental one (drop occurs), but the one that behaves differently indicates so high force comparing to the others, that when I summarize the NFORCes, I get the increasing tendency.
I have used quadratic 8 node elements for this FEA.
I think the model itself is somehow OK, I probably do something wrong when evaluating the results. I would welcome any suggestion.
Thank you very much.
I have modeled axisymmetric analysis of sheet dome (simple push button).
I need to get the force response of the sheet metal. According to experimental results the force increases until certain level then the "spring" action occurs and the force drops a little bit and if you keep "pushing the button", the force increases very much. I am concerned about the force drop range.
However I keep getting steadily increasing force curve from the surface nodes (NFORC). Actually except one node all indicates the behavior similar to the experimental one (drop occurs), but the one that behaves differently indicates so high force comparing to the others, that when I summarize the NFORCes, I get the increasing tendency.
I have used quadratic 8 node elements for this FEA.
I think the model itself is somehow OK, I probably do something wrong when evaluating the results. I would welcome any suggestion.