2 face plates (different thicknesses; 24mm and 28mm) of same longitudinal are butt joint, and the joint is ground flush.

Fatigue point of view; what are the consequences? My perception suggests that it is always reccomended to have a proper welding geometry (i.e. max 3mm depth of welding profile measured from the top of the face plate to the top of the weld)

Any ideas?

Gokhan
 
Replies continue below

Recommended for you

Use a 3:1 minimum taper for the thickness transition and blend grind the weld cap flush to remove any local stress concentration.
 