I'm looking for the flow curve for the following material:
Material number: 1.1117
Symbol: 8Mn4 ,respectively.

Anyone has any idea?

In common: where can I such flow curves get from?

Thanks for suggestions!

Best regards,
WoKu
 
Replies continue below

Recommended for you

What do you mean by flow curves? Do you mean typical stress-strain curves as produced during ambient temperature tensile testing? Or do you want data on flow stresses at various temperatures, usually presented as stress-strain "flow curves". These types of flow curves also depend greatly on the strain rate, so that is another variable to consider.

I do not have either of these curves for this alloy. Some places to look would be the following:

Atlas of Stress-Strain Curves from ASM International

Hot Working Guide: A Compendium of Processing Maps


 