Is there any methods/tips to improve the flatness of machined G10?
The raw material's dimension is around 360mm*360mm*2.0mm, the target thickness for milling is 1.0mm. After that, it will part off to a circular disc with O.D. of 320mm.
Significant "bowl up" effect was observed (>0.30mm). Is there any way to improve the flatness, my target is (<=0.10mm).
Thanks.
The raw material's dimension is around 360mm*360mm*2.0mm, the target thickness for milling is 1.0mm. After that, it will part off to a circular disc with O.D. of 320mm.
Significant "bowl up" effect was observed (>0.30mm). Is there any way to improve the flatness, my target is (<=0.10mm).
Thanks.