Dear all,
Ihave tested 80/100penetration grade bitumen materials for surface dressing according to AASHTO M20-70(1993)and the test results achieved are as follows
uctility at 25C,cm=>100-passed,penetration value,mm=92-passed,FLASH POINT=312-failed,Solubility in trichloroethylene=99.9-passed,Loss on heating<0.1=passed.Is it possible to allow the Contractor to use the bitumen materials,because all the rest of the test have passed except the flash point which failed.Does it be a critical issue or I have to reject the bitumen materials?
Ihave tested 80/100penetration grade bitumen materials for surface dressing according to AASHTO M20-70(1993)and the test results achieved are as follows