Flaring in Stainless Steel 5D Pipe Bends

Status
Not open for further replies.

hirendhara1234

Mechanical
May 9, 2009
5

In 10"x Sch 40 5D Pipe bends (Material SA 403 Type 304L ) if flaring is observed at end portions is it acceptable? what is acceptable criteria for flaring?
 
Replies continue below

Recommended for you

Look up Table 4 in ASME SA 106 for diameter tolerances. There is not such term as 'acceptable flaring'.
Cheers,
gr2vessels
 