Jun 23, 2007 #1 redandysafc Mechanical Joined Dec 18, 2005 Messages 60 Location GB Can anybody tell me were I would get a astm number for all fittings on 316,316L 304 and 304L. I think that forgings are A182 and fittings are Astm 403 . But can somebody put me on the right track please.
Can anybody tell me were I would get a astm number for all fittings on 316,316L 304 and 304L. I think that forgings are A182 and fittings are Astm 403 . But can somebody put me on the right track please.
Jun 23, 2007 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Yes. The product form information below is from Table 1 in ASME B16.34, which is referenced by ASME B16.11, which is the Specification for fittings ASTM A 182 forged/forged bar ASTM A 240 plate ASTM A 479 bar ASTM A 430 Tubular ASTM A 376 " ASTM A 358 " ASTM A 312 " Upvote 0 Downvote
Yes. The product form information below is from Table 1 in ASME B16.34, which is referenced by ASME B16.11, which is the Specification for fittings ASTM A 182 forged/forged bar ASTM A 240 plate ASTM A 479 bar ASTM A 430 Tubular ASTM A 376 " ASTM A 358 " ASTM A 312 "
Jun 27, 2007 1 #3 GRoStruc Marine/Ocean Joined Oct 11, 2006 Messages 23 A good cross reference for Stainless steels and various standards can be found here: http://www.ssina.com/publications/specs.html You can view, but to get a print-able copy you need to fill out a short survey. I never had any contact/spam from doing this. Upvote 0 Downvote
A good cross reference for Stainless steels and various standards can be found here: http://www.ssina.com/publications/specs.html You can view, but to get a print-able copy you need to fill out a short survey. I never had any contact/spam from doing this.