I'm trying to determine the possiblility of creating a storage attic in my garage. My trusses are Fink Style with the following specs:
28' span
9/12 pitch
2x4 truss construction
Lumber specs: S-Dry, SPF, 2100 Fb 1.8E, Machine rated 201
Connector Plates are 4x4 (6x4 at the center splice joint)
My questions are:
Can a 5/8 subfloor be safely installed for light storage?
Can any reinforcing of the existing truss system be performed? (plywood gussets??)
If light storage is feasible, where is the best place to locate the loads? (Down the center or towards the bearing walls?)
Thanks in advance for your help!
28' span
9/12 pitch
2x4 truss construction
Lumber specs: S-Dry, SPF, 2100 Fb 1.8E, Machine rated 201
Connector Plates are 4x4 (6x4 at the center splice joint)
My questions are:
Can a 5/8 subfloor be safely installed for light storage?
Can any reinforcing of the existing truss system be performed? (plywood gussets??)
If light storage is feasible, where is the best place to locate the loads? (Down the center or towards the bearing walls?)
Thanks in advance for your help!