ASME II C, at SFA 5.28 addresses this somewhat but doesn't address the suffix "R". AWS A5.5 address this as low-hydrogen electrodes. From what I see, this is a 2.25CR/1MO used in a cold climate for equipment with high temp and high pressure application. Also that pre-heat and interpass temps are critical and post weld heat treat is required.
what I would like to know is can I substitute this tig wire in other applications and would I need to requalify the PQR for any and all substituted applications?
This is a new plant for me and I found a large supply of this in stock. I am not familiar with this filler.
what I would like to know is can I substitute this tig wire in other applications and would I need to requalify the PQR for any and all substituted applications?
This is a new plant for me and I found a large supply of this in stock. I am not familiar with this filler.