Does anyone know where I can find a design example that shows the analysis process when using a fiber wrap on a concrete beam repair?
 
Agree with it being done by the mfr in my experience. We gave them the amount of rebar, strength of rebar, and assumed rebar depth it would take which they then took and turned into an equivalent amount of wrap. They submitted calcs for our review as well.
 
Thanks for the information.
 
Following references may be consulted for relevant material and examples;

1. Reinforced Concrete Design with FRP Composites by Gangarao et al.

2. Strengthening and rehabilitaion of civil infrastru using FRP composites by Hollaway and Teng
 
I have this book and find it to be full of useful examples: Link

Flexural or shear reinforcing? I might have a MathCAD worksheet from a homework assignment.

The greatest trick that bond stress ever pulled was convincing the world it didn't exist.
 